That's the first coat of tool coat applied, with particular attention to over hangs. Generally I mix up about 100 grams and put it into tight corners like where the part meets the parting board first while it still flows like no tomorrow. Once it starts to get a little thicker I move onto vertical walls, overhangs and the like.

I'll let this set up for an hour or two, and then I'll give it a second coat of tooling epoxy. I'm shooting for about 1/16" thick and complete coverage.

Haha - my tool ID tag fell off, but both bulldog tags stayed put - can't win for losing. I'll stick the tool ID tag on later I guess.